O que este vídeo aborda

Adriano Plotzky repairs localized osmosis blisters on the hull of his boat, Balanço, by sanding down to the gelcoat and drying the laminate.0:14 Although no blisters were visible before sanding, the process revealed small, vinegar-scented droplets trapped in the fiberglass.0:18 To identify moisture levels, he uses a 160-real moisture meter purchased in Curitiba, which allows him to compare relative humidity across different hull sections.0:40 Because the meter lacks specific fiberglass calibration, he uses it to pinpoint areas requiring targeted drying rather than relying on absolute percentage readings.0:47 To accelerate the drying process in cooler weather, he constructs a plastic greenhouse enclosure around the hull to trap solar heat.1:36 After cleaning the opened blisters with acetone and a hair dryer, he fills the voids with a mixture of epoxy resin, hardener in a 60-40 ratio, and fiberglass microspheres.3:12 He uses a scale to ensure precise mixing ratios and applies the filler with a spatula, later sanding the cured patches flush.3:45

Ver no YouTube

Mais de Hashtag Sal

The First Sailing Trip of 4 Guys from Minas: A Complete Disaster09/2026They Sold Everything and Headed Straight for the Anchor | #SAL #43609/2026The Social Project Teaching the New Generation of Sailors | #SAL #74 Clip09/2026This Was the Last Sailing of a Chapter in My Life | #SAIL #43409/2026

De Hashtag Sal — veja o barco, a tripulação e todos os vídeos analisados do canal.

The Sailing Directory Newsletter

Um email com os melhores achados da frota — os momentos, barcos e histórias que valem o seu tempo de visualização. Insira o seu endereço para receber a sua cópia.

Reportar um problema