Bertram Transom Mystery Solved / I Knew Better But Made The Wrong Choice

11 maggio 2025 · 16 min · 21K visualizzazioni

Cosa tratta questo video

Polyester gel coat applied to a boat transom failed to cure, leaving a tacky, unworkable surface that gummed up sandpaper.1:47 Troubleshooting revealed the issue was not expired gel coat or catalyst, but insufficient film thickness caused by using a thick-nap roller.5:10 Polyester resins require a minimum film thickness of approximately 20 mils to cure properly; the heavy-nap roller spread the material too thinly to fill the texture of the 1708 fiberglass cloth.6:37 To resolve the failure, the surface was cleaned with a dedicated de-waxer—as acetone does not effectively remove wax—and recoated with a fresh, thicker layer of gel coat applied with a short-nap mohair roller.10:55 Testing confirmed that applying the material more liberally allowed it to cure fully.14:33 The primary takeaway is that gel coat application requires a short-nap roller or brush to ensure adequate thickness, and any questionable materials should be verified with a small test batch before application to the boat.

Guarda su YouTube

Altro da BoatworksToday

Will This Entire Victron Electrical System Fit In My Little Boat?ago 2026The Primer Mistake You're Probably Making Painting Your Boat: Film Thickness, Not Smoothness!ago 2026V-Berth Electrical Layout On A Small Sailboat: It's Tight, But It Should Work!ago 2026Putting the Anona Orbis Solar Camera to Work on My Property ~ 360 Security Cameralug 2026

Da BoatworksToday — guarda la barca, l'equipaggio e ogni video analizzato del canale.

The Sailing Directory Newsletter

Una email con le migliori scoperte della flotta — i momenti, le barche e le storie che meritano il tuo tempo di visione. Inserisci il tuo indirizzo per riceverne una copia.

Segnala un problema