BoatworksTodayvídeo

Bertram Transom Mystery Solved / I Knew Better But Made The Wrong Choice

11 de maio de 2025 · 16 min · 21K visualizações

O que este vídeo aborda

Polyester gel coat applied to a boat transom failed to cure, leaving a tacky, unworkable surface that gummed up sandpaper.1:47 Troubleshooting revealed the issue was not expired gel coat or catalyst, but insufficient film thickness caused by using a thick-nap roller.5:10 Polyester resins require a minimum film thickness of approximately 20 mils to cure properly; the heavy-nap roller spread the material too thinly to fill the texture of the 1708 fiberglass cloth.6:37 To resolve the failure, the surface was cleaned with a dedicated de-waxer—as acetone does not effectively remove wax—and recoated with a fresh, thicker layer of gel coat applied with a short-nap mohair roller.10:55 Testing confirmed that applying the material more liberally allowed it to cure fully.14:33 The primary takeaway is that gel coat application requires a short-nap roller or brush to ensure adequate thickness, and any questionable materials should be verified with a small test batch before application to the boat.

Ver no YouTube

Mais de BoatworksToday

Will This Entire Victron Electrical System Fit In My Little Boat?08/2026The Primer Mistake You're Probably Making Painting Your Boat: Film Thickness, Not Smoothness!08/2026V-Berth Electrical Layout On A Small Sailboat: It's Tight, But It Should Work!08/2026Putting the Anona Orbis Solar Camera to Work on My Property ~ 360 Security Camera07/2026

De BoatworksToday — veja o barco, a tripulação e todos os vídeos analisados do canal.

The Sailing Directory Newsletter

Um email com os melhores achados da frota — os momentos, barcos e histórias que valem o seu tempo de visualização. Insira o seu endereço para receber a sua cópia.

Reportar um problema