Sail Life - Coppercoat antifouling - DIY sailboat refit

26 de agosto de 2018 · 23 min · 90K visualizações

O que este vídeo aborda

Applying Coppercoat antifouling to the hull of the sailboat Athena requires extensive surface preparation, including removing amine blush from the previous barrier coat and sanding the entire hull to ensure a mechanical bond.1:12 Before application, the crew must repair pinholes in the fairing compound by drilling them out and filling them with thickened epoxy.3:58 The Coppercoat process involves mixing resin, hardener, and copper powder, ideally at temperatures between 20 and 25 degrees Celsius to improve workability.8:31 Using a team of four, the crew applied six coats to the hull, averaging one hour per coat.14:07 The product requires a final abrasion step three to four days after application to expose the copper particles encapsulated in the epoxy.20:08 While the initial cost is higher than traditional antifouling, the long-term expense is lower for liveaboards who avoid annual haul-outs.16:15 Proper preparation and a multi-person team significantly simplify the labor-intensive application process.

Assistir no YouTube

Barcos neste vídeo

Antares Yachts 44O barco deles

Mais de Sail Life

The road back to boat work: Bunker roof, done! Ep. 699out. de 2026The road back to boat work: A bunker surprise. Ep. 698out. de 2026BUNKER vs. LASER - xTool MetalFab laser welder and CNC Ep. 697set. de 2026The road back to boat work: Bunker Makeover! Ep. 696set. de 2026

De Sail Life — veja o barco, a tripulação e cada vídeo analisado do canal.

The Sailing Directory Newsletter

Um e-mail com os melhores achados da frota — os momentos, barcos e histórias que valem o seu tempo de visualização. Insira seu endereço para receber sua própria cópia.

Reportar um problema